Have a part made of 17-4ph. Will receive (2) [solid bar]
handles welded to it so that it will look like a "T" configuration. Plan to weld first, then heat treat, then grind. Passivation in Citric Acid is planned as the final operation. Normal rinse is plain old clean water - no sodium dichromate or any other types of rinses are normallly part of our process. Do we need to be concerned about any possible future localized attack in the welded area arising from the passivation process following the welding?
handles welded to it so that it will look like a "T" configuration. Plan to weld first, then heat treat, then grind. Passivation in Citric Acid is planned as the final operation. Normal rinse is plain old clean water - no sodium dichromate or any other types of rinses are normallly part of our process. Do we need to be concerned about any possible future localized attack in the welded area arising from the passivation process following the welding?