Is passivation effective on high tensile strength, (>270ksi), quenched and tempered modified 420ss?

Our customer is using the material as as flexure strap on a power washer, the assembly is the SS strap clamped btw a galvanized plate, and a 380 Al casting. eventually the crevices begin to show some corrosion ruining the highly prepared surface and causing fatigue failure initiation and subsequent failure.

Chemistry of MOD420SS:

C: 0.36-0.40%
Si: 0.30-0.50%
Mn: 0.45-0.65%
P: MAX 0.025%
S: MAX 0.010%
Cr: 13.2-13.8%
Mo: 0.90-1.10%

This is a special SS melted in small heats and with extremely low inclusion counts. We stamp the parts from ~HRc 50 coil and then do some edge/surface finishing in order to increse the fatigue life. Our custome asked if passivation would help prevent the corrosion from starting.

Will it?

MY thoughts: redesign or change materials since this steel is barely stainless.

nick
 
Passivation will help, but may only delay the inevitable. Try it first, as it is less expensive than redesigning.

Federal spec. QQ-P-35C shows a Type II passivation for 420 SS. This consists of 20+ minutes in a 2.5 wt% sodium dichromate dihydrate + 20-25 vol.% nitric acid (67 wt% nitric acid basis) at 120-130oF. Note: QQ-P-35C is obsolete but still frequently used, and is free at
Stellar Solutions has versions of their citric acid-based product suitable for martensitic SS passivation per ASTM A967. Lee Kremer is a helpful guy:

In a redesign, perhaps chromate & powdercoat both plate & casting.
 