Hello,
I have a 410 CRES drawing note along with a heat treating note, and need advice on which passivation spec to use. I first used QQ-P-35 which is obsolete, which is my bad. They change it without notifying me to MIL-DTL-5002 which I believe is wrong. It think it should be per AMS 2700 which is specific to cleaning CRES. The MIL-DTL-5002 seems to generalize with processing al type of materials. Is this an incorrect statement?

Thanks a bunch,

Colin Fitzpatrick (aka Macduff)
Mechanical Designer
Solidworks 2010 SP 5.0
Dell T5500 Windows 7 Pro (64-bit)
Xeon CPU 2.53 GHz 6.00 GB of RAM
nVida Quadro 4000 2 GB
3D Connexion-SpaceExplorer
 
Replies continue below

Recommended for you

We call up AMS 2700 when appropriate, and 5 years or so ago did some research to justify why.

Sadly I can no longer remember any details.

Posting guidelines faq731-376 (probably not aimed specifically at you)
What is Engineering anyway: faq1088-1484
 
I have used all of them in the past.
From my experience, the companies that we have used to do the passivation know and understand MIL-DTL-5002 more often.

Chris