For a vessel constructed to ASME Sec VIII Div 1, where a nozzle reinforcing pad will be made from a dished head, and that head will be made from two pieces of plate, welded together by the head vendor, is a PDR form necessary? The repad will not be pressure retaining in itself, as it is vented, however, it seems it will still be subjected to stress( indirectly) induced by pressure? Am I thinking right here?