Dear all
We have a CrMoV turbine casing with a large crack (35 mm depth). We have come to the conclusion that we do not want a full weld repair because of distoration concerns. We believe that it would be acceptable to leave the crack in situ as it is below the crical size.
The cracking is associated with original weld repairs of the casting which possibly was not heat treated correctly after repair.
We are currenlty discussing a partial weld repair (say 10 mm depth).
Any thoughts or experience?
We have a CrMoV turbine casing with a large crack (35 mm depth). We have come to the conclusion that we do not want a full weld repair because of distoration concerns. We believe that it would be acceptable to leave the crack in situ as it is below the crical size.
The cracking is associated with original weld repairs of the casting which possibly was not heat treated correctly after repair.
We are currenlty discussing a partial weld repair (say 10 mm depth).
Any thoughts or experience?