This is a crosspost from r/StructuralEngineering on Reddit.
Link to reddit post
Link to follow up post from reddit OP
Link to photos (also posted below)
Looks like reddit OP made a subreddit for this which includes more photos.
Photo credit goes to Reddit user u/One-Truth-5867
According to the reddit OP this was photographed in the parking deck below a 6-story building hotel. But some google mapping it appears that this is not under the building but in the parking deck adjacent to the building. So, the the damaged portion of this column appears to be supporting only one level at the top level of the garage. Photo 'evidence' at the bottom of this post.
The OP has reported this to the building department and they are aware of the "issue".
Location:
The Falls Hotel & Inn
5657 Victoria Ave, Niagara Falls, ON.
My guess would be some sort of thermal expansion of the decks that would be opposing each other? Doesn't look great, but better than being a main building column. Discuss!
Link to reddit post
Link to follow up post from reddit OP
Link to photos (also posted below)
Looks like reddit OP made a subreddit for this which includes more photos.
Photo credit goes to Reddit user u/One-Truth-5867
According to the reddit OP this was photographed in the parking deck below a 6-story building hotel. But some google mapping it appears that this is not under the building but in the parking deck adjacent to the building. So, the the damaged portion of this column appears to be supporting only one level at the top level of the garage. Photo 'evidence' at the bottom of this post.
The OP has reported this to the building department and they are aware of the "issue".
Location:
The Falls Hotel & Inn
5657 Victoria Ave, Niagara Falls, ON.
My guess would be some sort of thermal expansion of the decks that would be opposing each other? Doesn't look great, but better than being a main building column. Discuss!