Hi,
I want to model the compression of a polymer cylinder. For that purpose, I want to use a linear Drucker Prager yield criterion with no hardening and a non-associative flow rule.
I have seen that in Abaqus the linear Drucker Prager requires the introduction of three parameters: friction angle, flow stress ratio and dilation angle.
The flow stress ratio I will set it to 1, assuming that the yield surface in the deviatoric plane is a circle.
I know the value of friction angle from other experiments. Also I have the value of the compression yield stress.
Therefore, my question is: how can I calculate the value of dilation angle from the parameters that I have, i. e. friction angle and compression yield stress? Is it possible?
Thank you in advance!
I want to model the compression of a polymer cylinder. For that purpose, I want to use a linear Drucker Prager yield criterion with no hardening and a non-associative flow rule.
I have seen that in Abaqus the linear Drucker Prager requires the introduction of three parameters: friction angle, flow stress ratio and dilation angle.
The flow stress ratio I will set it to 1, assuming that the yield surface in the deviatoric plane is a circle.
I know the value of friction angle from other experiments. Also I have the value of the compression yield stress.
Therefore, my question is: how can I calculate the value of dilation angle from the parameters that I have, i. e. friction angle and compression yield stress? Is it possible?
Thank you in advance!