Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Paragraph 5.7.4.6

Status
Not open for further replies.

MJEZ8

Mechanical
Joined
Feb 28, 2015
Messages
1
Location
AE
Gentlement

Kindly explain to what is all about?
5.7.4.6 When used in stress-relieved assemblies, the material of quenched and tempered steels A537, CL 2, and A678, Grade B, and of TMCP steel A841 shall be represented by test specimens that have been subjected to the same heat treatment as that used for the stress relieved assembly.

Thank you in advance...
 
To assure that the material meets the mechanical properties with the added heat treatment during construction.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top