Feb 3, 2003 #1 AVIATOR2 Industrial Joined Feb 3, 2003 Messages 1 Location US Problem: Wire feed burning back to the tip at arc end sequence. The problem is intermittant. Have adjusted AES voltages, replaced tips, running 92/8 gas mixture. Welding 16 gage mild steel tube.
Problem: Wire feed burning back to the tip at arc end sequence. The problem is intermittant. Have adjusted AES voltages, replaced tips, running 92/8 gas mixture. Welding 16 gage mild steel tube.
Mar 23, 2003 #2 RTRANT Industrial Joined Mar 23, 2003 Messages 3 Location US CHECK GAS OFF DELAY CHECK WIRE FEED OFF DELAY CHECK LINER FOR GRABBING WIRE (ARE THERE WAVES IN WELDED AREAS) Upvote 0 Downvote
CHECK GAS OFF DELAY CHECK WIRE FEED OFF DELAY CHECK LINER FOR GRABBING WIRE (ARE THERE WAVES IN WELDED AREAS)
May 12, 2005 #3 abnrml1 Automotive Joined Apr 8, 2003 Messages 5 Location US 90 % of the time its the liner getting gunked up... try installing a wire kleener pad by Lube-Matic before it goes into the wire feeder should increase liner life and reduce burn back. Upvote 0 Downvote
90 % of the time its the liner getting gunked up... try installing a wire kleener pad by Lube-Matic before it goes into the wire feeder should increase liner life and reduce burn back.