Hi Guys,
I have just had a question put to me from one of our customers and I am not sure how to answer it!
We supplied them some P91 pipe spools where the welds were PWHT'd for 2 hours per our qualified WPS. Our customer has now added attachments to these spools and now needs to PWHT their welds, This is all good but they have asked me if its OK to PWHT the full spool in a furnace.
I have never encountered this before and my first reaction is to say no as it will mean our welds go through a second PWHT cycle which was not qualified by our PQR. My gut feeling is to tell them that their welds need to be locally PWHT'd.
So.... what do you guys think?
Thanks
I have just had a question put to me from one of our customers and I am not sure how to answer it!
We supplied them some P91 pipe spools where the welds were PWHT'd for 2 hours per our qualified WPS. Our customer has now added attachments to these spools and now needs to PWHT their welds, This is all good but they have asked me if its OK to PWHT the full spool in a furnace.
I have never encountered this before and my first reaction is to say no as it will mean our welds go through a second PWHT cycle which was not qualified by our PQR. My gut feeling is to tell them that their welds need to be locally PWHT'd.
So.... what do you guys think?