P355 GH is Equivalent to SA 516GR60 OR SA516GR70

Status
Not open for further replies.

yaar123

Mechanical
Sep 1, 2014
19
P355 GH is Equivalent to SA 516GR60 OR SA516GR70????????
 
Replies continue below

Recommended for you

SA/EN 10028–2 P355GH is in ASME Section II, part D, and it is similar to SA 516 Gr 70. I don't like the word "equivalent" because that means interchangeable. Review the stress lines for each to be sure.
 