Hi all,

Could anyone help me in finding door seal manufacturers for freezing chamber? The temperature range is -70 to room temp in celcius. so far silicone rubber is my choice of material (teflon might be a little overkill). I couldn't find anyone selling stocked extruded silicone gasket (P shape profile).

any suggestions are welcomed!

Thanks!!

Lee
 
Replies continue below

Recommended for you

Gaskets, Inc. makes a number of tadpole gaskets. My catalog has some silicone tadpole samples. You can contact them through this website:

 