Jan 12, 2021 #1 johnlabuu Petroleum Joined Sep 10, 2017 Messages 8 Location MY Dear Friends, Should someone advise me, what is the P Number for material P335 P36? Thank You. Johnlabu
Dear Friends, Should someone advise me, what is the P Number for material P335 P36? Thank You. Johnlabu
Jan 12, 2021 #2 XL83NL Mechanical Joined Mar 3, 2011 Messages 3,115 Location NL What is P335 P36 for kind of material? What standard does it complies to? So you have any more info? Huub - You never get what you expect, you only get what you inspect. Upvote 0 Downvote
What is P335 P36 for kind of material? What standard does it complies to? So you have any more info? Huub - You never get what you expect, you only get what you inspect.
Jan 12, 2021 #3 goutam_freelance Mechanical Joined Jan 25, 2003 Messages 649 Location IN The A335 P36 P no is not defined. Welding has to have special procedure and undergo special procedure qualification. Refer Table A2 of B31.1. Engineers, think what we have done to the environment !https://www.linkedin.com/in/goutam-das-59743b30/ Upvote 0 Downvote
The A335 P36 P no is not defined. Welding has to have special procedure and undergo special procedure qualification. Refer Table A2 of B31.1. Engineers, think what we have done to the environment !https://www.linkedin.com/in/goutam-das-59743b30/