Dear All,

I have to qualify two welding procedures involving following base materials

1)one WPS for A995 GR 4A (UNASSIGNED) to A182 F51 (P No. 10 H Gr 1)

2)one WPS for A995 GR 4A (UNASSIGNED) to A995 GR 4A (UNASSIGNED)

Are both WPS qualified by a PQR in which base materials are
A995 GR 4A (UNASSIGNED) to A240 UNS S31803 (P No. 10 H Gr 1)?

Thank you for your help

Marco
 
Replies continue below

Recommended for you

Marco,
You should be posting in the ASME section.
The answer to your question is no, you will require two PQRs (QW 424),
Regards,
Kiwi
 