This is a major question for which you have supplied no process or failure data. Without process description or data, you are unlikely to get much help in finding the underlying problem.
With respect to oxygen sources, what about water? Cooling water or steam leaks into the process can lead to corrosion issues. Following the water trail can often lead to effective corrosion mitigation.
The best start to finding the source of corrosion is to cut out the failed section for metallurgical analysis. Is this pitting, general thinning, crevices, deposits, heat affected zones, etc? If you know nothing about the failures then the chance of finding the cause is very low. Let an expert take his microscope to the problem and do some elemental analysis of the corrosion products.
good luck,