Anyone who has data (e.g. corrosion rates) on oxygen corrosion due to high dissolved oxygen in boiler feed water?
 
Replies continue below

Recommended for you

EPRI document 1017482 may be useful. Otherwise find someone that has both a DO analyzer and corrosion product monitor.
 
Thank you, MFJewell and metengr. Do you know any other references from API, NACE or ASME regarding this? I cannot see any established corrosion rates as functions of temperature, DO, pressure and velocity.
 
EPRI is where these experts would publish paper since it is power generation focused.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
I Andijani, S Turgoose, Prediction of oxygen induced corrosion in industrial waters, Water Science and Technology, Vol 49, (2), 2004, pp 115-120.

Steve Jones