After 1 nos of boiler superheater tube replacement, we conducted hydrotest. the test pressure is 1.5 x MAWP= 71 Bar. But due to mistake in chart recorder, we overpressured it till 122 bar.
We depressured it and performed visual inspection to see if the overpressure caused any deformation. But there was non found. So we redo the hydrotest with correct test pressure of 71 bar, and we found that 1nos of tube (different from the 1 we replaced) is leaking at the superheater header to tube weldment.
My question is, could the tube leak due to the overpressure or the tube is already defect before that. Is there a way to know what caused the tube leak. The original tube we replaced also because of the defect in the weldment.
All the other tubes are fine with no trace of leak at 71bar.
Thank you
We depressured it and performed visual inspection to see if the overpressure caused any deformation. But there was non found. So we redo the hydrotest with correct test pressure of 71 bar, and we found that 1nos of tube (different from the 1 we replaced) is leaking at the superheater header to tube weldment.
My question is, could the tube leak due to the overpressure or the tube is already defect before that. Is there a way to know what caused the tube leak. The original tube we replaced also because of the defect in the weldment.
All the other tubes are fine with no trace of leak at 71bar.
Thank you