what UPAS stan for? I got the following description of an overhead line
1 x 132kV, 300mm2 "UPAS"
kind regards
iigp2006
 
Replies continue below

Recommended for you

This is one cable code name for 19 strand aluminum alloy conductor.

This OH cable code name is use in the IEC marketplaces such as UK and Australia.
 