Honestly I think there are lots of problems i dont know where to begin with our cranes.
On this particular crane a drive wheel outer flange recently collapsed after what looks like excessive wearing and allowed the wheel to roll over the rail onto the opposite side. I have just been up and checked the wheel diagnoally opposite it also has wear on its outer flange well past the 50% allowance
It suggests to me skewing. I also believe im hearing lots of creaking and popping noises which I havent noticed before.
I want to be in a position to diagnose problems properly and suggest the proper solutions.
Ive been told the rails were recently realigned so that shouldnt be the issue. Id like to check the drive assembly for backlash that would cause skew as I believe the issue could be routed in here. I believe the wheel diameters should be checked but im unsure how to do this accurately.