Hi all,
I am planning to use Iridite 7p per MIL-C-5541 to coat my copper waveguide. The issue is that those waveguides have to go in a thermal vacuum chamber so the outgassing of the coating must be low.
Does anyone know if that coating has already been used for a space application and where I could find some outgassing data (I went to the NASA website but nothing is there).
Best regards,
Franck
I am planning to use Iridite 7p per MIL-C-5541 to coat my copper waveguide. The issue is that those waveguides have to go in a thermal vacuum chamber so the outgassing of the coating must be low.
Does anyone know if that coating has already been used for a space application and where I could find some outgassing data (I went to the NASA website but nothing is there).
Best regards,
Franck