Hello,
I’ve seen out-of-roundness defined various ways depending on the standard. Can anyone please help me interpret the out-of-roundness per ASTM A358 (Electric Fusion Welded Stainless Steel Pipe) stating:
“Out-of-Roundness – difference between major and minor outside diameters, 1%.”
Is this similar to ASME Sec VIII Div UG-80; where Out-of-Roundness is defined as: (Major Outside Diameter – Minor Outside Diameter) / Nominal Outside Diameter?
I’ve seen out-of-roundness defined various ways depending on the standard. Can anyone please help me interpret the out-of-roundness per ASTM A358 (Electric Fusion Welded Stainless Steel Pipe) stating:
“Out-of-Roundness – difference between major and minor outside diameters, 1%.”
Is this similar to ASME Sec VIII Div UG-80; where Out-of-Roundness is defined as: (Major Outside Diameter – Minor Outside Diameter) / Nominal Outside Diameter?