I am analyzing a composite (carbon/epoxy) component.
For the Hashin-fabric failure criterion (see attachment), some out of plane properties are needed.
We do not have time for coupon testing.
Specific materials are:
- Standard Modulus Carbon fibre fabric 5H Satin 370 g/m²
- Liquid Epoxy Resin 180°C curing RTM6
Available properties/allowables from spec are (MPa):
E11=67000, E22=67000, G12=4700, NU12=0.2
Xt=730 --> actual warp allowable is 750 but weft allowable is used for both warp and weft.
Xc=630
Yt=730
Yc=630
S12=70
Guessed values are (MPa):
E33=4500, G12=1600, G23=1600, NU13=0.4, NU23=0.4
Zt=58 --> tensile strength UD-fabric in weft direction @RT
Zc=170 --> compressive strength UD-fabric in weft @RT
S13=UNKNOWN
S23=UNKNOWN
Are the guessed values realistic and how can I derive the missing properties/allowables?
Any help is appreciated.
Best Regards,
Tom
For the Hashin-fabric failure criterion (see attachment), some out of plane properties are needed.
We do not have time for coupon testing.
Specific materials are:
- Standard Modulus Carbon fibre fabric 5H Satin 370 g/m²
- Liquid Epoxy Resin 180°C curing RTM6
Available properties/allowables from spec are (MPa):
E11=67000, E22=67000, G12=4700, NU12=0.2
Xt=730 --> actual warp allowable is 750 but weft allowable is used for both warp and weft.
Xc=630
Yt=730
Yc=630
S12=70
Guessed values are (MPa):
E33=4500, G12=1600, G23=1600, NU13=0.4, NU23=0.4
Zt=58 --> tensile strength UD-fabric in weft direction @RT
Zc=170 --> compressive strength UD-fabric in weft @RT
S13=UNKNOWN
S23=UNKNOWN
Are the guessed values realistic and how can I derive the missing properties/allowables?
Any help is appreciated.
Best Regards,
Tom