I've seen there is an old thread about removing orange peel from surfaces, but my question is different. I've noticed many cars, even new and from premium manufacturers, say MB, have orange peel all over the paint finish, and it's clearly visible. Now, that wasn't the case some 15-20 years ago, if I remember well. I'm curious what is the reason for this kind of paint finish, even with premium manufacturers? I guess it has to do something with water based paint, but what is the exact cause? Faster thinner evaporation, different paint applying techniques, or something else?