Hello Everybody!

I've some trouble with aircraft cleaning. IAW Boeing AMM we have to use cleaner alkaline MIL-PRF-87937, but could you please advise any optional commercially available compound for MIL-PRF-87937?

Thank you.

Roman
 
Romanos
I am listing some materials and suppliers that claim to meet the requirements of MIL-PRF-87937. You can check the claims and acceptability with your client.

ALK-660 -- manufacturer claims it conforms to the MIL-PRF-87937 Type II spec.
[][]
Same manufacturer claims Astrosol Orange meets Type 1 of the spec and that Astrosol 37 meets Type III of the spec.

Zip Chem: Calla 804 (Ty IV); Calla Solve 120 (TY 1, not authorized for final surface prep prior to paint or sealant;
Calla 800 (TY II)

Spray 9: AV-8 (TY IV)
[][]
 
bchoate,

thank you for this info, it's really useful for me!
 