Oct 25, 2003 #1 SPLIT Mechanical Joined Dec 21, 2002 Messages 57 Location CL Optimum Ratio H/R for atmosferic tanks API 650 ?
Nov 24, 2003 #2 MrVessels Mechanical Joined Jan 30, 2003 Messages 13 Location GB Tables A-1a/b and A-3a/b of API 650 Appendix A gives optimum sizes of tanks up to 66m or 220ft dia based on course heights of standard plates of 1800mm/72inches or 2400mm/96inches. Upvote 0 Downvote
Tables A-1a/b and A-3a/b of API 650 Appendix A gives optimum sizes of tanks up to 66m or 220ft dia based on course heights of standard plates of 1800mm/72inches or 2400mm/96inches.