Oct 29, 2003 #1 beercia Mechanical Joined Jul 11, 2003 Messages 36 Is it allowed by code to have the reinforcing plate of manhole opening overlap an horizontal shell course weld? Carlos
Is it allowed by code to have the reinforcing plate of manhole opening overlap an horizontal shell course weld? Carlos
Oct 29, 2003 #2 IFRs Petroleum Joined Nov 22, 2002 Messages 4,679 Location US I think the answer for API 650 tanks is: Yes as long as the reinforcing pad intersects the horizontal weld at 90 degrees and extends past the horizontal weld by 6" if the shell plate is less than 1/2" thick and (the greater of 10" and 8T) if greater than 1/2" thick. Upvote 0 Downvote
I think the answer for API 650 tanks is: Yes as long as the reinforcing pad intersects the horizontal weld at 90 degrees and extends past the horizontal weld by 6" if the shell plate is less than 1/2" thick and (the greater of 10" and 8T) if greater than 1/2" thick.