Does anyone have any spec's for this material R301W I belive it was a Reynolds product. It was used by Repbublic Aviation in the late 40's. What I'm looking for is a material to replace the 301.
 
The document you need is called ANC-5. This is the predecessor of Mil-Hnbk-5 and MMPDS. I have a hard copy of this and looked up R301 for you. The new designation is 2014 clad. I think the W is a heat treat condition (I could be way off on this). W condition is unstable (right after quench). The ANC-5 document lists R301-T6 sheet and plate per QQ-A-255. Ftu-65 L-dir, .040-.499 thk, A-basis, Fty-58, Fcy-58, Fsu-39, Fbru-98 1.5ed, Fbry-81, E-10.4, Ec-10.6.

Sorry but I couldn't find an internet source for ANC-5.

Hope this helps. If you need more info let me know.
 
Thanks Kwan
I'll have a look at ANC-5.
 