Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Old Steel Section Properties 4

Status
Not open for further replies.

engcom

Structural
Jul 7, 2003
15
Does anyone know where I find section properties for W6 X 15.5. The steel section is no longer in the modern AISC Manuals.
 
Replies continue below

Recommended for you

There is a FAQ in this forum regarding that kind of information.

Several 6" by 15.5 are listed in the AISC Iron and Steel Beams 1873 to 1952.

You may wish to check out slideruleera.net for such out of print texts and references.

Regards,
Qshake
[pipe]
Eng-Tips Forums:Real Solutions for Real Problems Really Quick.
 
I found a WF6x15.5 in an old Bethlehm Steel catalog from 1948. A=4.62 d=6.00 b=6.00 tf=0.269 tw=0.240 I=30.3 S=10.1 r=2.56 fillet radius=0.30, flange faces are parallel
 
Qshake: Where is there an FAQ? I didn't know there were any...
 
nutte:

click on the FAQ tab on top of this page, Qshake has a post there related to this topic.
 
Ahh, thanks. I had never noticed the FAQs tab.
 
Library: HISTORIC
Type: WF
ID = 169
Designation = 6WF
W = 15.5
A = 4.62
D = 6
TW = 0.24
BF = 6
TF = 0.269
T = 4.737
K = 0.632
BF_2TF = 11.15
H_TW = 19.7
FY3P = -
X1 = 2913
X2 = 1954
IX = 30.3
ZX = 11
SX = 10.1
RX = 2.56
IY = 9.7
ZY = 4.9
SY = 3.2
RY = 1.45
J = 0.12
CW = 79
a = 42
WNO = 8.6
SW = 3.47
QF = 2.22
QW = 5.52
FSTR = 6W(B6) 6x6 ,S53 1943, 6 WF(B6) 6x6 ,S54 1946,S56 1948,
 