Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Old Channel Properties

Status
Not open for further replies.

diverseengineer

Civil/Environmental
Joined
Jan 12, 2012
Messages
1
Location
US
I am looking for section properties on what is being called out as a channel (" [7x3.5 BSC-10 20.3# ") on a set of lattice tower plans. The plans are dated 1958.

Thanks for your efforts in advance.



 
according to an old carnegie steel manual i have that's a british standard section ship building channel. from the designation you can probably figure out that it's 7" deep with a 3.5" wide flange and weighs 20.3 plf. other properties are:

area of section = 5.9 in^2
web thickness = 0.400 in
strong axis I = 44.2 in^4, r = 2.74 in, s = 12.6 in^3
weak axis I = 6.7 in^4, r = 1.07 in, s = 2.8 in^3, y = 1.09 in