Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

oil contamination in soil for offshore pile design

Status
Not open for further replies.

saeed_1980

Geotechnical
Sep 12, 2022
1
During drilling a 110m offshore borehole, the existence of soil layers containing active hydrocarbon materials was investigated which a phenomenon is almost rare in geotechnical studies (the depth 60m up to end of borehole). The in-situ CPTU, sampling and experimental tests on undisturbed soil was performed.
Considering the limitations in the standards and similar experiences regarding soil contaminated with crude oil:
• Are there any standards which in defined soil-crude oil interaction in geotechnics?
• How to utilize the reduction factor on deep foundation design parameters including ultimate capacity, P-y, T-z, Q-z and SRD curves? The pile is OD= 60” thickness= 1” length= 85m and some part of pile will be penetrated in oily contaminated soil.
• What is the effect of contamination to mobilize shaft resistance in piles?
11_gagy4m.jpg
 
Replies continue below

Recommended for you

If its very oily and contaminated (whats very oily?:)) I would imagine that it is reducing the strength of the material. But how do you quantify this. You run tests on the samples you have, but then the next question is, are the samples representative of the material.