Dear Eng-tips Members,

I have been looking for some in-sight with 'Eqivalent Total Combustible Gas' percentage calculation , when it comes to interpreting results of a transformer oil test report.

I was wondering if there is a particular formula that is used to calculate this parameter?

Thank you.
 
Replies continue below

Recommended for you

IEEE C57.104 shows the equation in section 6.3

It is hard to reproduce in this forum.