Dear all,
Currently I'm working as inspector on the following pressure vessel:
Pressure vessel designed acc. to ASME VIII Div.2 2017 Cl.2, material SA 533 Type C Cl.2.
This vessel has a shell and an ellipsoidal head 2:1.
+Shell: I.D. 3670mm Nom.Thk. 42mm
+Head: I.D. 3658mm Nom.Thk. 38mm
From my calculations I find the following:
CL offset: 8mm ; OD Misalignment: 10mm ; ID Misalignment: 6mm
According to ASME VIII Div.2 2017 Par.6.6.5.4 "Joint alignment", is not clear to me the definition of Joint alignment in this case. Have I to use CL offset as reference or have I to apply the same tolerance for CL, OD Misalignment and ID Misalignment? Should Table 6.4 be applicable only for OD Misalignment and ID Misalignment?
I think that ASME VIII Div.1 it's more understandable in this case.
Regards
Theo

 
Replies continue below

Recommended for you

What is your judgment as an inspector?

Regards
 
Dear r6155,
Definetely Not Conform, according to ASME VIII Div.2 2017 Par.6.6.5.4 for thk>38mm the tolerance is 12,5% of the thickness but max 6mm.
Regards
 
This occurs when rolling the shell before receiving the head, or a certified dimensional report.

Regards
 