...The reports clearly show that many batteries have been inadequately tested before being put on sale. Problems have included:
- Difficulty physically installing and connecting batteries.
- Problems with communication between batteries and inverters.
- Parts vital for installation that are not “off the shelf” haven’t been supplied with batteries.
- Instructions for installation were often not included with batteries or were inadequate.
- The majority were not delivered on time.
- Testing has shown some batteries losing capacity or “fading” rapidly. This may result in many future warranty claims for currently installed battery systems.
One area identified as being desperately required is standardised protocols for communication between batteries and inverters....