Working on an aluminum boat. Need to know how much zinc to put on. What current density should I use for calculation?
5- ? -30 (mA/m^2)
Boat will be sand blasted and painted with Proline polyurethane paint. Will be in salt water.

Any sources would be useful.

thanks,