Ok, here goes:
We have new customer who has specified a part in nylon 6.6.
We have the contract and during the sign-off meeting they mentioned that the parts are bolted onto a galvanized steel part. The end use is a truck curtain sided trailer - non critical application.
I mentioned than Zn salts and nylon (why it's specified as 6.6, rather then 6 I have no idea!) are generally a no-no due to esc blah blah blah...
Has anyone actually experienced a failure to to nylon being in contact with Zn in the real world?
Cheers
Harry
We have new customer who has specified a part in nylon 6.6.
We have the contract and during the sign-off meeting they mentioned that the parts are bolted onto a galvanized steel part. The end use is a truck curtain sided trailer - non critical application.
I mentioned than Zn salts and nylon (why it's specified as 6.6, rather then 6 I have no idea!) are generally a no-no due to esc blah blah blah...
Has anyone actually experienced a failure to to nylon being in contact with Zn in the real world?
Cheers
Harry