Any suggestions on how to weld these two pipes together? (picture attached)
 
Replies continue below

Recommended for you

First, adjust your cope so that the intersecting tube saddles better. You have a large gap in the top joint visible and it looks like a knife edge in the side joint. A good cope will change both conditions. The knife edge will then offer a shoulder with mass enough to help prevent burn through. Second, the actual weld process in indeterminate from your jpg. Not knowing the material involved makes the wildest SWAG impossible.
 