How do your nuc tests on average compare with the sand cone results on average? The strength of nuclear gauge testing is that even though an individual test may vary from a theoretical "correct" value more than a sand cone test, the nuclear density results can more accurately represent the whole of the material represented because it is practical to take many more tests using the nuclear method rather than using the sand cone method.
The phenomenon that Ron mentions regarding deflection of radiation occurs with non-metallic materials as well. In fact, though we measure the overall density of a sample, a sample contains materials of varying densities and the shape and orientation of the various particles can affect an individual test result. I find that when the overall average density is marginal when compared with a modified proctor or Gmm (for asphalt), the variability of the nuclear gauge results as measured by the standard deviation is greater, often much greater, than material compacted on average a few points above the minimum. However, as long as you have statistically valid sample sizes, the average difference between nuclear results and sand cone results remains very close to the same regardless of whether the material is marginally or well compacted and regardless of the increased standard deviation of the nuc results in marginally compacted materials.
I would be very surprised if the above did not hold true in materials containing metallic metals as well. Even if metallic particles are more likely to deflect radiation, that would result in a greater amount of variation in nuclear test results, but should not invalidate them as long as you have adequate sample size. In addition, we think of "metallic" materials as reflective based on our experience, but that is a property of a material exposed to visible light. Gamma emissions from a cesium 137 source is another matter.
I suppose all of the above goes out the window if the material being tested contains a gamma-emitting element that will be measured by the densometer.