Hello friends
my customer requirement PWHT, NOTCH TOUGHNESS .
I have welding procedure which have PWHT BUT NO notch toughness test.
please guide me.
stanly.
 
stanly3164, also known as Charpy impact test, see ASME SA-370 or ISO 148

Regards,

Mike

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 
Notch Toughness or Charpy Impact Test is a supplementary essential variable as per Sec-IX when called for by the design code(Sec VIII Div-1 & others).Addition or deletion of an essential variable calls for requalification of procedure.
Thus a new PQR is needed.
If you stick the same PQR regime: same base metal( preferably with same CE), welding consumables, welding parameters, PWHT cycle, [highlight #FCE94F]only an impact test could be used an addendum to the existing PQR.[/highlight].

Thanks.

Pradip Goswami,P.Eng.IWE