Sorry folks but free Fe ions, suphuric acids, oxide layers etc. aren't my forte so I have a pretty basic question.
I got a vendor looking for a concession. Our spec asked for the vessel to be grit blasted and pickled......oops they didn't pickle but bead blasted only. Can we accept?
Now I would think the bead blast would accomplish pretty much what you were looking the acid bathing to do for the vessel, right? Get rid of all scale, embedded contaminants, give a "clean" surface to epoxy the outside with and provide the best carbon steel surface to resist corrosion.
Our process fluid is demin water.
Is there something crucial I'll need the pickling for here or was I over-specified (not my TS)
Frank "Grimey" Grimes
Rule 25. of Swanson's "Unwritten Rules of Management"
Have fun at what you do. It will reflect in your work. No one likes a grump except another grump.
I got a vendor looking for a concession. Our spec asked for the vessel to be grit blasted and pickled......oops they didn't pickle but bead blasted only. Can we accept?
Now I would think the bead blast would accomplish pretty much what you were looking the acid bathing to do for the vessel, right? Get rid of all scale, embedded contaminants, give a "clean" surface to epoxy the outside with and provide the best carbon steel surface to resist corrosion.
Our process fluid is demin water.
Is there something crucial I'll need the pickling for here or was I over-specified (not my TS)