I have a norwegian reinforcement drawing from 1975 and I am trying to get an understanding on what a couple of things mean:
Kontrollklasse: Utivdet
Betongkvalitet: C45
Stalkvalitet: Ks40
A Norwegian friend translated it for me to mean:
Control Class : Expansion
Concrete Quality: C45
Steel Quality: Ks40.
My query is more related to norwegian practice.
1] C45 in the UK means a 28 day cube strength of 45 MPa. The europeans tend to use cylinder strength instead of cube strength. Does this mean in this instance C45 is a cylinder strength?
2] Does anyone know what Ks40 means in terms of rebar grade. 400 MPa yield perhaps?
Any help would be appreciated.
---------------------------------------------------------------------------------------------------------------------
![[pimp] [pimp] [pimp]](/data/assets/smilies/pimp.gif)
"The world keeps turning, it keeps me in my place; where I stand is only three miles from space"
Spiritualized
Kontrollklasse: Utivdet
Betongkvalitet: C45
Stalkvalitet: Ks40
A Norwegian friend translated it for me to mean:
Control Class : Expansion
Concrete Quality: C45
Steel Quality: Ks40.
My query is more related to norwegian practice.
1] C45 in the UK means a 28 day cube strength of 45 MPa. The europeans tend to use cylinder strength instead of cube strength. Does this mean in this instance C45 is a cylinder strength?
2] Does anyone know what Ks40 means in terms of rebar grade. 400 MPa yield perhaps?
Any help would be appreciated.
---------------------------------------------------------------------------------------------------------------------