Nov 22, 2005 #1 repairguy Aerospace Joined Jan 21, 2005 Messages 2 Location CA Can anyone telll me if there is a North American Eqivalent for E-Z20WC10 / RBD Modified Composition is 85Fe/3Cr/0.7Ni/0.2C/0.3Mn/0.4V/10W
Can anyone telll me if there is a North American Eqivalent for E-Z20WC10 / RBD Modified Composition is 85Fe/3Cr/0.7Ni/0.2C/0.3Mn/0.4V/10W
Nov 23, 2005 #2 EdStainless Materials Joined May 20, 2004 Messages 16,366 Location Waukesha WI USA Are you off a litle on the carbon? H-21, H-22, H-23 type hot work tool steels are actually very close. = = = = = = = = = = = = = = = = = = = = Corrosion, every where, all the time. Manage it or it will manage you. http://www.trent-tube.com/contact/Tech_Assist.cfm Upvote 0 Downvote
Are you off a litle on the carbon? H-21, H-22, H-23 type hot work tool steels are actually very close. = = = = = = = = = = = = = = = = = = = = Corrosion, every where, all the time. Manage it or it will manage you. http://www.trent-tube.com/contact/Tech_Assist.cfm