Hello,
Can anyone tell me an equivalent European standard grade for stainless steel to Norsok standard M-630 MDS D45. Left to my own devices I would subscribe to one of the materials databases or buy reference book on the subject but my new company is reluctant to spend money on such things.
 
Replies continue below

Recommended for you

Thank you metalonis for your prompt reply, will try my supplier with this info and see if it helps,

Regards
 
It is not equivalent to, it ACTUALLY is ASTM A240 UNS S31803 and S32205. It says so at the top of the datasheet.

Steve Jones
Materials & Corrosion Engineer
 