Hello all
i have clad plate of (40+5 mm) sa-516 gr 70 + sa-240 317 . We are giving that plate for dished end manufacturing , cold forming
My vendor say that he will do normalizing of cold form dish end at 910°C for 1 hr 10 min .
my question is what will happen to ss-317 plate if heated at 910°C . will this temperature will tear down the clad bonding also .
Is S.R is not enough 610°C for 1 hr 45 min . As per ASME code i am not bale to find any such data .
i have clad plate of (40+5 mm) sa-516 gr 70 + sa-240 317 . We are giving that plate for dished end manufacturing , cold forming
My vendor say that he will do normalizing of cold form dish end at 910°C for 1 hr 10 min .
my question is what will happen to ss-317 plate if heated at 910°C . will this temperature will tear down the clad bonding also .
Is S.R is not enough 610°C for 1 hr 45 min . As per ASME code i am not bale to find any such data .