Under ASME Section VIII Division 1 what is the benefit, if any, of specifying normalized steel for standard B16.5 flanges?
I have searched Eng-Tips and seen that others have had the same question. There's been discussion of this issue (as in thread292-16359) but there seems to be no satisfying answer, at least in terms of Code references.
Normalizing is often applied for the purpose of improving notch toughness and impact test properties, and consequently the ability to operate at lower design temperatures (or MDMT). But under ASME Section VIII Division 1 the rated MDMT of standard B16.5 flanges is not a function of the material but rather of the flange pressure-temperature rating as per UCS-66(b)(1)(b). Thus specifying normalizing (when not otherwise required) doesn't gain anything in the MDMT rating.
ASTM material specification A-105 paragraph 5.1 requires normalizing for standard flanges over Class 300 so specifying "N" for such flanges should not be required as the manufacturer should do this anyway.
So, is there any need at all to specifically call out normalized B16.5 flanges for an ASME Section VIII Division pressure vessel?
I have searched Eng-Tips and seen that others have had the same question. There's been discussion of this issue (as in thread292-16359) but there seems to be no satisfying answer, at least in terms of Code references.
Normalizing is often applied for the purpose of improving notch toughness and impact test properties, and consequently the ability to operate at lower design temperatures (or MDMT). But under ASME Section VIII Division 1 the rated MDMT of standard B16.5 flanges is not a function of the material but rather of the flange pressure-temperature rating as per UCS-66(b)(1)(b). Thus specifying normalizing (when not otherwise required) doesn't gain anything in the MDMT rating.
ASTM material specification A-105 paragraph 5.1 requires normalizing for standard flanges over Class 300 so specifying "N" for such flanges should not be required as the manufacturer should do this anyway.
So, is there any need at all to specifically call out normalized B16.5 flanges for an ASME Section VIII Division pressure vessel?