The title of the post is severe cyclic, which requires 100% RT or UT. However, many people misclassify systems as severe cyclic. But if it is in fact severe cyclic, the 100% RT or UT requirements only apply to those portions of the system that are severe cyclic, that is, where the calculated stress due to thermal expansion and other displacement loading is over 80% of the allowable (+ more than 7000 cycles). The 5% part and the 100% parts are treated entirely seperately with respect to examination.