I'm just wondering while researching about non-shrink grout. Can one make an entire beam or column using non-shrink grout instead of poured concrete? What is its disadvantage aside from price? What is the equivalent aggregate sizes of non-shrink grout, 3/4" or 1" or is it equal to ready-mix concrete of finer aggregates?
 
Replies continue below

Recommended for you

In short, you can't afford it. Properly designed concrete will work fine for almost every application. If needed, you can specify shrinkage-compensating concrete.
 
pre-packaged high strength, non-shrink grout generally does not have any coarse aggregate, only sand. it can sometimes be mixed with up to 3/8 inch rock for grouting large voids, but that will perform differently than ordinary 3/4 or 1 inch mix concrete. I can't think of a good reason to do what you suggest not to mention the much higher cost.
 