Hi all,
Our client in the middle east has specified an 14" API 5L X60 with a wall thickness of 55 mm (minimum), i.e nominal around 60mm
In accordance with Table 9 on API 5L 45th Ed our pipe doesn't fall under the "Permissible specified outside diameter and specified wall thickness" therefore our potential manufacturers have advised that they can't apply the API monogram (but still will comply with API requirements anyway)
Is there a way to go round that table and still get the pipe monogrammed? if not, what are the potential risks of procuring that pipe?
Awaiting replies,
Our client in the middle east has specified an 14" API 5L X60 with a wall thickness of 55 mm (minimum), i.e nominal around 60mm
In accordance with Table 9 on API 5L 45th Ed our pipe doesn't fall under the "Permissible specified outside diameter and specified wall thickness" therefore our potential manufacturers have advised that they can't apply the API monogram (but still will comply with API requirements anyway)
Is there a way to go round that table and still get the pipe monogrammed? if not, what are the potential risks of procuring that pipe?
Awaiting replies,