Hi every body,

I am looking for a new non-contact 3d profilometer for our inspection station. Does anybody have an idea about a provider?

I am trying to measure the surface roughness of reflective steel using a non-contact 3d profilometer. I am having problems due to the reflectiveness of the finish. I heard white light profilometers have a very hard time unless some spray is applied. Do other technologies (ie: LCI non contact 3d profilometers ) have better results?

Thanks a lot.

 
We have had success at 2 microinch Ra with white light interferometers (have not tried a lower Ra than that). Veeco and Zygo are two companies that serve this application.

 