Hi- I'm hoping for some help on locating an odd material spec. I need to find someone that manufactures a high-tensile strength (1500 psi)buna-n that is non-conductive (no carbon-black fillers or other conductive fillers). Anyone out there know where I can find it? Rest of the details- 60 duro, 300% elongation, 25% comp set.
 
Hello,
any good custom compounder should be able to provide
you with white Buna-N or any other white Nitrile
compound. White Nitriles are without carbon blacks
and are a very common compound for all rubber goods which
are used in the food industry.
We use white Nitrile for oil resistant cable sheating
and have typical Rv values of > 10power9 Ohms.

Best Regards