Does anyone know of any problems with using Nitronic 50 stems in boiler feed water valves operating around 200°F?
 
I don't see any problem with using N50 at your conditions. I would use the 1950F annealed material.

I've used N50 and N60 all around boiler feed water pumps and valves.
 